xfnano
High conductivity graphene/carbon nanotube composite slurry
Product Name
Name:High conductivity graphene/carbon nanotube composite slurry
Product Overview
High conductivity carbide graphene/carbon nanotube composite slurry is a conductive slurry that combines the excellent properties of graphene and carbon nanotubes (CNTs)
Technical Parameter
Carbon content:9.5±0.5 wt%
Additive content:1±0.1wt%
Solvent:Water
Conductivity:400-600 S/cm
Viscosity:¡ãC000 mPa.s
Granularity:D50 ï½?13um
D90 ï½?49um
Lateral size:5-15 um
Thickness:2-5 nm
OD:5-15 nm
Length::0 um
Note:The above is a single measurement data,the test results of different batches fluctuated. The viscosity of the dispersion increases with time.
Product Features
High solid content can fully utilize the role of graphene, providing conductivity, heat dissipation, and anti-corrosion effects.
High conductivity, coating conductivity can reach 400-600 s/cm.
High viscosity, slow settling, easy to apply.
Good dispersibility, mechanical stirring can re disperse.
Application Fields
Lithium batteries: Graphene/carbon nanotube composite conductive paste has a wide range of applications in the field of lithium batteries, especially for lithium iron phosphate batteries, which can significantly reduce battery internal resistance, improve rate performance and cycle life.
Flexible electronics: Due to its high conductivity and good mechanical properties, this composite paste is also suitable for the manufacturing of flexible electronic products, such as flexible sensors, flexible displays, etc.
Energy storage devices: In energy storage devices such as supercapacitors and battery energy storage systems, high conductivity carbide graphene/carbon nanotube composite slurry can enhance the overall performance of the devices.
Conductive coatings and adhesives: can be used to prepare conductive coatings and adhesives, widely used in fields such as electronics, construction, and automotive.
Related Information
Sealed, avoid light, away from spark and heat, and keep at normal temperature. Expiry date: Six months before unsealing. Please use it as soon as possible upon opening. Precipitation may form if placed for a long time. Shake or stir it before using.
Please e-mail for the detailed characterization data.
E-mail:sales@xfnano.com